1. Ọjọgbọn ti a lo fun aṣọ-ikele odi ti kii ṣe ipilẹ-ipilẹ ati fifẹ docking, pẹlu gilasi, awo aluminiomu, awo ṣiṣu aluminiomu, ara ẹya ara ati awọn miiran ti o ga-jinde Aṣọ odi oju ojo lilẹ.
2. Oju ojo lilẹ ni irin (ko pẹlu Ejò), gilasi, okuta, aluminiomu nronu, ati ṣiṣu
3. Igbẹpọ idapọ ati awọn ibeere aabo ti o ni idi pupọ.
1. Ẹya-ara kan, didoju-ni arowoto pẹlu ifaramọ ti o dara julọ, oju ojo ati elasticity fun lilẹ oju ojo ni aṣọ-ikele ati awọn facades ile;
2. O tayọ oju ojo ati giga resistance si ultraviolet Ìtọjú, ooru ati ọriniinitutu, ozone ati awọn iwọn otutu;
3. Pẹlu ifaramọ ti o dara ati ibamu pẹlu ọpọlọpọ awọn ohun elo ile;
4. Duro rọ lori iwọn otutu ti -400C si 1500C;
5. Koju awọn ipo ayika ti o lagbara gẹgẹbi ikojọpọ afẹfẹ, ojo ti afẹfẹ afẹfẹ, egbon ati sleet.
1. Mọ pẹlu awọn nkanmimu gẹgẹbi toluene tabi acetone lati jẹ ki awọn aaye sobusitireti di mimọ ati ki o gbẹ;
2. Fun ideri irisi ti o dara julọ ni ita awọn agbegbe apapọ pẹlu awọn taps masking ṣaaju ohun elo;
3. Ge nozzle to fẹ iwọn ati ki o extrudes sealant si awọn agbegbe isẹpo;
4. Ọpa lẹsẹkẹsẹ lẹhin ohun elo sealant ati ki o yọ teepu masking ṣaaju ki o to awọn awọ ara.
1. Mọ pẹlu awọn nkanmimu gẹgẹbi toluene tabi acetone lati jẹ ki awọn aaye sobusitireti di mimọ ati ki o gbẹ;
2. Fun ideri irisi ti o dara julọ ni ita awọn agbegbe apapọ pẹlu awọn taps masking ṣaaju ohun elo;
3. Ge nozzle to fẹ iwọn ati ki o extrudes sealant si awọn agbegbe isẹpo;
4. Ọpa lẹsẹkẹsẹ lẹhin ohun elo sealant ati ki o yọ teepu masking ṣaaju ki o to awọn awọ ara;
5. Ọja ifasilẹ oju ojo iṣẹ Ere pataki ti a ṣe apẹrẹ fun glazing gbogbogbo ati lilẹ oju ojo ni odi aṣọ-ikele ati awọn facades ile.
Igbesi aye ipamọ: 12osuif tọju edidi, ati fipamọ ni isalẹ 270C ni itura,dry ibi lẹhin ti awọn ọjọ ti gbóògì.
Iwọnwọn:GB/T 14683-mo-Gw-50HM
Iwọn didun:300ml
Awọn data atẹle jẹ fun idi itọkasi nikan, kii ṣe ipinnu fun lilo ni sipesifikesonu murasilẹ.
OLV4800 Silikoni Weatherproofing Building Sealant | ||||
Iṣẹ ṣiṣe | Standard | Idiwon Iye | Ọna Idanwo | |
Idanwo ni 50± 5% RH ati iwọn otutu 23± 2℃: | ||||
Ìwúwo (g/cm3) | ±0.1 | 1.37 | GB/T 13477 | |
Àkókò Ọ̀fẹ́ Awọ (iṣẹ́jú) | ≤180 | 20 | GB/T 13477 | |
Extrusion (milimita/iṣẹju) | ≥150 | 350 | GB/T 13477 | |
Modulu fifẹ (Mpa) | 23 ℃ | ﹥0.4 | 0.52 | GB/T 13477 |
–20℃ | or ﹥0.6 | / | ||
Slumpability (mm) inaro | ko yipada apẹrẹ | ko yipada apẹrẹ | GB/T 13477 | |
Slumpability (mm) petele | ≤3 | 0 | GB/T 13477 | |
Iyara Itọju (mm/d) | 2 | 3.5 | / | |
Bi Itọju - Lẹhin awọn ọjọ 21 ni 50 ± 5% RH ati iwọn otutu 23 ± 2 ℃: | ||||
Lile (Ekun A) | 20 ~ 60 | 35 | GB/T 531 | |
Agbara Fifẹ labẹ Awọn ipo Didara (Mpa) | / | 0.6 | GB/T 13477 | |
Ilọsiwaju ti Rupture (%) | / | 400 | GB/T 13477 | |
Agbara gbigbe (%) | 25 | 50 | GB/T 13477 | |
Ibi ipamọ | 12 osu |